title: EPU 40
slug: materials/epu-40
description: Discover the exceptional properties of EPU 40, a highly elastic and tear-resistant material perfect for vibration isolation, gaskets, and seals.
docTags: 
createdAt: 2024-06-28T18:14:50.310Z
---

# Overview

::::VerticalSplit{layout="middle"}
:::VerticalSplitItem
**Highly elastic, tear resistant, and resilient**

EPU 40 offers a combination of tear strength, moderate energy return/damping, and elongation making it perfect for vibration isolation, gaskets, and seals. It is a good choice for applications where high elasticity and tear resistance are needed. It is comparable to commercial TPUs with a Shore A hardness of 70.
:::

:::VerticalSplitItem
![EPU 40 Example](https://res.cloudinary.com/carbon3d/image/upload/Education/Materials/elastomer/EPU-40/epu-40-button-pad.png)
:::
::::

# Resource Links

::::LinkArray{contentSource="CUSTOM"}
:::LinkArrayItem{headerType="IMAGE" headerImage="https://api.archbee.com/api/optimize/dptYqcTHPbVZhe3zuNg4v-yZnHZ5VDqzKJosZJznLXm-20241119-021407.png"}
**[About the Material
](https://www.carbon3d.com/materials/epu-40)**&#x4D;aterial overview and uses cases &#x20;
:::

:::LinkArrayItem{headerType="IMAGE" headerImage="https://api.archbee.com/api/optimize/3CesIL2dYMCHPZvRjp8S0/meEa1m4VN4HOvIJpjIIld-20251016-220433.jpg"}
**[Technical Data Sheet
](https://docs.carbon3d.com/files/technical-data-sheets/tds_carbon_epu-40.pdf)**&#x4D;echanical properties and data
:::

:::LinkArrayItem{headerType="IMAGE" headerImage="https://api.archbee.com/api/optimize/3CesIL2dYMCHPZvRjp8S0/1r3fpdvMUMFVZGfey2Tjn-20251016-221405.jpg"}
**[Safety Data Sheet](https://www.carbon3d.com/stewardship)**
*Login required*
:::
::::

# Protocol Sheet

This downloadable handout provides important usage information, including instructions about compatible hardware, storage, resin dispensing, washing and curing. Print it out and bring it into the lab.

::::VerticalSplit{layout="left"}
:::VerticalSplitItem
**English**
:::

:::VerticalSplitItem
::File{src="https://api.archbee.com/api/presign/3CesIL2dYMCHPZvRjp8S0/KynT7FGDXG04dffXfMrbc-20260115-212320.pdf" label="EPU 40 Protocol v0601.pdf"}
:::
::::

::::VerticalSplit{layout="left"}
:::VerticalSplitItem
**German/Deutsch**
:::

:::VerticalSplitItem
::File{src="https://api.archbee.com/api/presign/dptYqcTHPbVZhe3zuNg4v-iScjo7LNINMm14-22Ax96-20241122-213230.pdf" label="EPU 40 Protocol v0504_German-Deutsch.pdf"}
:::
::::

::::VerticalSplit{layout="left"}
:::VerticalSplitItem
**Spanish/Español&#x20;**
:::

:::VerticalSplitItem
::File{src="https://api.archbee.com/api/presign/dptYqcTHPbVZhe3zuNg4v-A3ts17V5I5oochvGEa5tI-20241122-213252.pdf" label="EPU 40 Protocol v0504_Spanish-Espanol.pdf"}
:::
::::

::::VerticalSplit{layout="left"}
:::VerticalSplitItem
**Japanese/日本語**
:::

:::VerticalSplitItem
::File{src="https://api.archbee.com/api/presign/dptYqcTHPbVZhe3zuNg4v-XOIyh0ybVtezl0eLrT6ai-20241122-213304.pdf" label="EPU 40 Protocol v0206_Japanese-日本語.pdf"}
:::
::::

# Thermal Processing

Some resins may crystallize or freeze at lower temperatures requiring a thermal processing step, also known as incubation, prior to dispensing.

:::hint{type="info"}
Reference this downloadable PDF for instructions.

::File{src="https://api.archbee.com/api/presign/3CesIL2dYMCHPZvRjp8S0/RARgfnxBS7FnQzm-evFYq-20260218-210534.pdf" label="Resin Thermal Processing v0502.pdf"}
:::